First, the iron ore mountains and rivers
The Tieshanhe iron ore deposit is a dolomite hydrothermal metasomatism magnetite deposit. The recoverable minerals include magnetite and pyrite. Since the cobalt- containing pyrite associated with the plant was not considered for recycling, the magnetic separation tailings of the plant were sieved and analyzed to a content of -0.074mm of 47.5%, including 3.6% sulfur and 0.065% cobalt. The same form exists in pyrite, and the other part exists in limonite, hematite, and maghemite. Cobalt in pyrite accounts for about 60%, cobalt in iron minerals accounts for about 15%, and cobalt in other gangues accounts for about 25%. Among the pure pyrite monomers, the highest cobalt content is 0.79%. A portion of the pyrite is oxidized to limonite. Under the light sheet, there is still a residue of pyrite in the limonite. Therefore, after research and examination, the heavy magnetic weight combined sorting process (see Figure 1) is used to recover the cobalt-containing pyrite in the magnetic separation tailings. The large-capacity GL600 spiral concentrator is used to terminate the tail and then magnetically removed. Magnetic magnetite and maghemite to facilitate subsequent shaker sorting, while reducing the inclusion of pyrite in the iron concentrate. 45,000 t annual processing tailings magnetic count, year can produce a sulfur-containing cobalt of greater than 0.5% above the drill 2500t concentrate containing cobalt metal 12.5t over annual profit of 100 million yuan.
Figure 1 selection process flow chart
Second, the Guangxi Beibu Bay Beach titanium ore
The favorable minerals of zircon , monazite and iron-bearing ferrous stone, which are comprehensively utilized in the Beibei Bay seashore ilmenite ore deposit, are associated. Small concentrators in Tiezhou and Fangcheng use dry magnetic separation to produce a single ilmenite product. The tailings still contain a large amount of useful minerals: fine-grained ilmenite 10%-20%, iron-bearing rutile 1% to 3% with anatase, 7% to 22% for zircon, 1% to 5% for monazite; secondly, tailings sand contains a large amount of quartz sand, a very small amount of tourmaline , leucox , garnet , Minerals such as biotite . The analysis of the tailings sand shows that the particle size is mostly between -0.2+0.05mm, and the monomer dissociation degree of the mineral is very ideal, and the living body is only occasionally seen. In order to achieve the purpose of comprehensive utilization, the plant adopts the heavy-floating-magnetic joint production process to separate and recycle the selected titanium tailings, and only increases the number of the original PC3×600 dry magnetic separator based on the selected plant. A 6-S fine sand shaker and a 3A single-slot flotation machine. The production process of the plant is shown in Figure 2.
Figure 2 Production process
The tailings are sorted by a shaker to discard most of the gangue minerals, so that the heavy minerals are enriched. At the same time, after the shaker is sorted, the clay wrapped on the heavy minerals is removed, and the minerals are exposed to the original organs. Provide conditions for subsequent flotation operations.
The flotation operation mixes zircon and monazite together, and as the next magnetic selection, the ilmenite and iron-bearing rutile are basically left in the flotation tailings. The particle size of the coarse concentrate into the float is below 0.2mm, and the concentration of the slurry is controlled at about 50% according to the level of the floating grade. Flotation can be carried out at normal temperature. Normal reagent system as follows: pH adjusting agent sodium 0.31kg / t, a commercially available soap (formulated as a 20% solution concentration) 0.15 ~ 0.03kg / t, coal oil collector 0.05 ~ 0.01kg / t, flotation Time: Stir for 7 min, rough for 12 min, sweep for 5 min. The flotation tailings are combined with the shaker mine, and a second shaker is selected to recover the coarser zircon and monazite.
The dried mixed concentrate is subjected to magnetic separation by PC3×600 dry three-plate magnetic separator, and a zircon qualified concentrate of (ZrHf)O 2 greater than 60% can be obtained by one magnetic separation, and the magnetic product is re-examined. A magnetic separation tailings is a monazite product (TR51%).
The process is used to select the heavy minerals in the tailings of the man-made wool after the selection of titanium, and at the same time obtain the qualified products of the titanium-containing products and the monazite, and the recovery rate of the zircon concentrate. High, high technical indicators, improve the comprehensive utilization of ore, and significantly improve the economic benefits of the plant.
Xinxiang SKF Machinery also supply grinding machine related consumables like Diamond Grinding Wheel and CBN Grinding Wheel.
Application fields:
1. Compressor parts: Cylinder, Piston, Slide, Valve plate,Roller sleeve, upper and lower bearings, etc;
2. Hydraulic parts: Blade in pump blade, stator and rotor in steering pump,gear ring, etc;
3. Blade:Hard alloy blade, high speed steel blade, etc;
4. Others:Magnetic parts, artificial gemstone, etc.
Grinding Plate,Super Hard Grinding Stone,Super Abrasive Grinding Plate,Dia Grinding Wheel
Xinxiang SKF machinery Co., Ltd. , https://www.grindingmachine.nl